4043 VS 4943 Advantage Comparison (Special Advantages of 4943 aluminum filler rod wire ): The 4943 aluminum filler rod wire does not need to rely on the elements that are rarefied by the base metal in the welding pool to improve the tensile
4043 VS 4943 Advantage Comparison (Special Advantages of 4943 aluminum filler rod wire):
The 4943 aluminum filler rod wire does not need to rely on the elements that are rarefied by the base metal in the welding pool to improve the tensile strength performance, while retaining all the advantages of the original 4043
• Good liquidity
• Low thermal fracture
• Low shrinkage
• Low melting point
• Good corrosion resistance
• Can be used in high temperature environment
• Low spatter of welding slag
• Tensile/shear strength is higher than 4043
• Heat treatable
Specifications of 4943 aluminum filler rod wire: 0.9mm, 1.0mm, 1.2mm
Application fields of 4943 aluminum filler rod wire:
Existing 4043 and 4643 welding workpieces, 1xxx, 3xxx, 5xxx (magnesium content <3.0%), 6xxx aluminum alloy base materials,
Heat-treated workpiece, cast aluminum A356, wheel rim, ladder frame/frame, furniture, daily repair (welding repair)
Aluminum alloy frame (bicycle, automobile, locomotive), aerospace hardware equipment, aluminum alloy ship deck
Mobile:86 17344894490
Email:inquiry@signialuminium.com